3L58 cold drawn and fully annealded soft wire rivet stock
|
BS 3L58(1971) Alloy 3L58 |
|
|---|---|
| Chemical Element | % Present |
| Aluminium (Al) | balance |
| Lead (Pb) | 0.05 max |
| Tin (Sn) | 0.05 max |
| Copper (Cu) | 0.1 max |
| Nickel (Ni) | 0.2 max |
| Zinc (Zn) | 0.2 max |
| Titanium + Zirconium (Ti+Zr) | 0.2 max |
| Chromium (Cr) | 0.25 max |
| Silicon (Si) | 0.3 max |
| Manganese (Mn) | 0.5 max |
| Manganese + Chromium (Mn+Cr) | 0.1 - 0.5 |
| Iron (Fe) | 0.5 max |
| Magnesium (Mg) | 4.5 - 5.5 |
Material shall be supplied annealed.
Aluminium alloy 3L58 - 5056A is covered by Standard BS EN 3L58 (1971)
The most common temper for 3L58 - 5056A aluminium rivet stock is cold drawn and fully annealed/fully soft
L58-5056A aluminium is supplied as cold drawn wire for rivet stock
|
BS 3L58(1971) Wire - |
|
|---|---|
| Mechanical Property | Value |
| Tensile Strength | 265 Min N/mm2 |
Material shall be subjected to a torsion test. This specification was declared obsolescent on 01 April 1999. It is susceptible to intergranular corrosion.